Diameters / Packaging
Diameters |
33# SPOOL |
---|---|
.035 | ED035144 |
.045 | ED035145 |
DETAILS
Blue Max® MIG wire is designed to perform exceptionally at high wire feed speeds
Features
- Designed to overlay mild and low alloy steels
- Preheat and inter-pass temperature of 300°F (150°C) or greater are recommended during welding
- Post-weld heat treatment should not exceed 1150°F (620°C) as higher temperatures may result in hardening
Typical Applications
- Turbines
- Power Generation
- Pressure Piping
Welding Positions
- All
Shielding Gas
- 98% Ar/ 2% O2
Disclaimers
Service Information
Documentation
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.9 | ER410NiMo |
WIRE COMPOSITION
Classification | %C | %Cr | %Cu | %Mn | %Mo | %N | %Nb | %Ni | %P | %S | %Si |
---|---|---|---|---|---|---|---|---|---|---|---|
ER410NiMo Requirement | 0.06 max. | 11.0 - 12.5 | 0.75 max. | 0.6 max. | 0.4 - 0.7 | 4.0 - 5.0 | 0.03 max. | 0.03 max. | 0.5 max. | ||
Typical Result | 0.02-0.03 | 11.8-12.1 | 0.04-0.06 | 0.4-0.5 | 0.5-0.6 | 0.02-0.05 | 0.00 max. | 4.5-4.7 | 0.01-0.02 | 0.01 max. | 0.4 |
TYPICAL OPERATING PROCEDURES
Diameter | Shielding Gas |
Voltage
volts |
Approx. Current
amps |
---|---|---|---|
0.035 in (0.9 mm) | 98% Ar / 2% O2 | 26-29 | 160-210 |
0.045 in (1.1 mm) | 98% Ar / 2% O2 | 28-32 | 180-250 |