Ultracore stainless, flux-cored wire, plastic spool

Diameters / Packaging

Diameters
50 lb Coil
500 lb Speed Feed® Drum
3/32 in (2.4 mm) ED035770 ED036620

UltraCore® 80Ni1M

Flux-Cored Gas-Shielded (FCAW-G)

CLASSIFICATIONS:
E80T1-Ni1M-JH8
E80T1-M21A4-Ni1-H8

UltraCore® 80Ni1C from Lincoln Electric has high deposition in the flat and horizontal positions.

DETAILS

High deposition in the flat and horizontal positions.

Features

  • High deposition in the flat and horizontal positions
  • Excellent operator appeal and slag detachability
  • Designed for welding with 75-80% Argon / balance CO2
  • ProTech® foil bag packaging

Typical Applications

  • Structural fabrication
  • Heavy equipment
  • Shipbuilding

Welding Positions

  • Flat/Horizontal

Shielding Gas

  • Mixed Shielding Gas

Disclaimers

Warning -

Cancer and Reproductive Harm -

www.P65Warnings.ca.gov

BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page

See test result disclaimer

MECHANICAL PROPERTIES

Classification Shielding Gas Polarity Yield Strength @ 0.2% Offset
MPa (ksi)
Tensile Strength
MPa (ksi)
Elongation
%
Charpy V-Notch
J (ft-lbs) @ -30°C (-20°F)
Charpy V-Notch
J (ft-lbs) @ -40°C (-40°F)
E80T1-Ni1M-JH8 Requirement 75-80% Ar, balance CO2 DC+ 470 (68) min. 550-690 (80-100) 19 min. 27 (20) min.
E80T1-M21A4-Ni1-H8 Requirement M21-ArC DC+ 470 (68) min. 550-690 (80-100) 19 min. 27 (20) min.
Typical Result, As-welded 75% Ar, 25% CO2 DC+ 550-600 (80-87) 620-660 (89-96) 25-28 66-122 (48-90) 28-92 (21-68)

DEPOSIT COMPOSITION

Classification Shielding Gas Polarity %B %C %Cr %Mn %Mo %Ni %P %S %Si %V Diffusible Hydrogen
mL/100g Weld Metal
E80T1-Ni1M-JH8 Requirement 75-80% Ar, balance CO2 DC+ 0.12 max. 0.15 max. 1.50 max. 0.35 max. 0.80 - 1.10 0.030 max. 0.030 max. 0.80 max. 0.05 max. 8.0 max.
E80T1-M21A4-Ni1-H8 Requirement M21-ArC DC+ 0.12 max. 0.15 max. 1.75 max. 0.35 max. 0.80 - 1.10 0.030 max. 0.030 max. 0.80 max. 0.05 max. 8 max.
Typical Result 75% Ar, 25% CO2 DC+ 0.002-0.005 0.04-0.08 0.06 max. 1.26-1.36 0.01 max. 0.84-1.04 0.012 max. 0.012 max. 0.48-0.61 0.02 2-8

TYPICAL OPERATING PROCEDURES

Diameter Shielding Gas Polarity CTWD
mm (in.)⁽¹⁾
Wire Feed Speed
m/min (in/min)
Voltage
volts
Approx. Current
amps
Melt-off Rate
kg/hr (lb/hr)
Deposition Rate
kg/hr (lb/hr)
Efficiency
%
3/32 in (2.4 mm) 75% Ar / 25% CO2 DC+ 25 (1) 3.2 (125) 27-32 340 5.4 (11.9) 4.7 (10.3) 87 - 89
3/32 in (2.4 mm) 75% Ar / 25% CO2 DC+ 31 (1 1/4) 5.1 (200) 27-32 465 8.6 (19.0) 7.6 (16.7) 87 - 89
3/32 in (2.4 mm) 75% Ar / 25% CO2 DC+ 31 (1 1/4) 6.4 (250) 30-36 620 13.1 (28.8) 11.4 (25.1) 87 - 89

NOTES

Note
⁽¹⁾ To estimate ESO, subtract 1/4 in. (6.0 mm) from CTWD.