Blue Max Stainless Wire

Diameters / Packaging

Diameters
33 lb Spool
0.035 in (0.9 mm) MG99035667
0.045 in (1.1 mm) MG99045667

Techalloy® 99

MIG (GMAW) | MG99035667

CLASSIFICATIONS:
AWS A5.15 : ERNi-CI

For cast iron joining and repair

DETAILS

Techalloy® offers a wide variety of nickel alloy grades of MIG, TIG, and SAW welding products lot tested with certificates of actual wire chemistry and typical mechanical results available online

Features

  • Welds produced are generally more machinable than a Tech-Rod® 55 deposit
  • A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks
  • Q2 Lot® - Certificate showing actual wire composition available online

Disclaimers

Warning -

Cancer and Reproductive Harm -

www.P65Warnings.ca.gov

BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page

See test result disclaimer

CONFORMANCE

CONFORMANCES SPECIFICATION CLASSIFICATION
AWS AWS A5.15 ERNi-CI

WIRE COMPOSITION

Classification %C %Fe %Mn %S %Si %Total Cu %Ni+Co
ERNi-CI Requirement 1.0 max. 4.0 max. 2.5 max. 0.03 max. 0.75 max. 4.0 max. 90 min.
Typical Result 0.0 0.1 0.0 max. 0.00 0.13-0.20 0.0 99

TYPICAL OPERATING PROCEDURES

Diameter Shielding Gas Polarity Voltage
volts
Approx. Current
amps
.035" (0.9 mm) 75% Ar, 25% He DC+ 24-27 150-190
.045" (1.1 mm) 75% Ar, 25% He DC+ 25-30 200-290