Diameters / Packaging
Diameters |
---|
Détails
Higher Silicon content 11-13 % with low melting point for excellent fluidity which also enables to be used as brazing alloy on thin sections.
Traits
- • Substitute for 4043 to increase Silicon in weld metal
- • Minimize hot cracking to produce higher fillet weld shear strength
- • Cosmetic appearing welds
- • Lower melting point and higher fluidity than 4043 wires
Positions de soudage
- All except vertical down
Gaz de protection
- 100% Argon Argon / Helium Mixtures Flow Rate: 30 - 50 CFH
Disclaimers
Des informations de service
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.10 | ER4047 |
WIRE COMPOSITION
Classification | %Be | %Cu | %Fe | %Mg | %Mn | %Si | %Zn |
---|---|---|---|---|---|---|---|
ER4047 Requirement | 0.0003 max. | 0.30 max. | 0.8 max. | 0.10 max. | 0.15 max. | 11.0 - 13.0 | 0.20 max. |
Typical Result | 0.0000 | 0.00 | 0.1 | 0.00 | 0.00 | 12.1 | 0.00 |