Diameters / Packaging
Diameters |
33 lb (15 kg) Steel Spool |
---|---|
0.035 in (0.9 mm) | MG55035667 |
0.045 in (1.1 mm) | MG55045667 |
DETAILS
TECHALLOY® 55 is ideal for a preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks.
Features
- The welds are moderately hard and require carbide tipped tools for machining
- A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks
- Q2 Lot® - certificates showing actual wire composition available online
Service Information
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
WIRE COMPOSITION
Classification | %C | %Cu | %Mn | %S | %Si | %Al | %Fe | %Ni+Co |
---|---|---|---|---|---|---|---|---|
Typical Result | 0.03 | 0.1 | 0.7 | 0.002 | 0.1 | 0.1 | 44.5 | 54.0 |
TYPICAL OPERATING PROCEDURES
Diameter | Shielding Gas | Polarity |
Voltage
volts |
Approx. Current
amps |
---|---|---|---|---|
0.9 mm (0.035 in) | 75% Ar / 25% He | DC+ | 26-29 | 150-190 |
1.1 mm (0.045 in) | 75% Ar / 25% He | DC+ | 28-32 | 180-220 |